TECHNICAL DATA SHEET

  ELECTROLESS NICKEL HARD CHROME
METAL DISTRIBUTION VERY GOOD POOR
CORROSION RESISTANCE 1,000 HOURS
ASTM B117
400 HOURS
ASTM B117
HARDNESS:
   AS DEPOSITED
   HEAT TREAT
  
48-52 Rc
70 Rc
  
64-69 Rc
48-52 Rc
MELTING POINT 1800oF 2900oF
WEAR RESISTANCE GOOD VERY GOOD
CO-EFFICIENT OF FRICTION:
   DYNAMIC
   STATIC
 
0.19
0.20
 
0.16
0.17
DUCTILITY 1-2% Very Low Almost 0
EFFLUENT COST RELATIVELY LOW HIGH
DEPOSITION RATE
(PER HOUR PER HOUR)
.0002 - .0003 .001 - .002
EFFECTIVE OF HYDROGEN EMBRITTLEMENT ON PLATED COMPONENTS FAIR/NOT SERIOUS USUALLY SERIOUS